Hello,
for my a10 i use
130 mm/s travel speed (but i'm going to try higer speed)
6000 mm/s retractation speed
A10M Stringing / Oozing (Same Settings - Different Results)
Re: A10M Stringing / Oozing (Same Settings - Different Results)
I use PTEG and did a lot of calibrations but still have oozing. Did removing little disks from the hotend will solve that problem?
Re: A10M Stringing / Oozing (Same Settings - Different Results)
This thread was quite helpful for me, I thought I'd try to contribute...
I'm curious to know if you found better solutions since the last post?
My suggestion at this point, given what I've seen so far, is that z-hopping should be the final solution to that pesky end-of-layer string if you can't get it fixed with retraction, temperature, speed, or altering the extruder path with combing, seam-hiding, etc.
I'm curious to know if you found better solutions since the last post?
My suggestion at this point, given what I've seen so far, is that z-hopping should be the final solution to that pesky end-of-layer string if you can't get it fixed with retraction, temperature, speed, or altering the extruder path with combing, seam-hiding, etc.