A10M Stringing / Oozing (Same Settings - Different Results)

Didi
Posts: 5
Joined: Tue Aug 27, 2019 4:52 pm

A10M Stringing / Oozing (Same Settings - Different Results)

Post by Didi » Tue Aug 27, 2019 5:20 pm

Hello,

One month ago, I bought the Geeetech A10M. From the Beginning i had bad stringing / oozing problems. In this forum i found the solution, which said to remove the little disks from the hotend. I removed them and started to find the best retraction settings. First i used two little 2mm cylinder which had a distance of 12mm. I found the best setting at 6mm by 40mm/s. Then i printed this controller grip and had bad stringing.

stringing switch controller.jpg
stringing switch controller.jpg (125.88 KiB) Viewed 13314 times

I decided to print another stringing test which had 10mm cylinder with distances 15mm, 30mm and 50mm. I startet with 1mm up to 11mm at 20mm/s. I found the range 7 to 9mm are the best. I increased the speed up to 25 and 30 mm/s.

string test 1.jpg
string test 1.jpg (216.06 KiB) Viewed 13314 times
string test 2.jpg
string test 2.jpg (222.82 KiB) Viewed 13314 times

Today i want to check if 8mm at 25mm/s is best and printed it again. but now i have stringng which is really bad. Here you can see both prints with 8mm at 25mm/s

8 25.jpg
8 25.jpg (338.07 KiB) Viewed 13314 times

Can anybody helb me? I have no idea what i can do now. What cold be the reaseon, why i have different results with the same settings?

Thank you
Didi

User avatar
William
Site Admin
Posts: 6340
Joined: Tue Jun 07, 2016 9:38 am

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by William » Tue Aug 27, 2019 5:29 pm

Hi, The drawback distance is recommended at 4-6mm,
The pumping speed can be tried at 20-40mm/s;
It is recommended that the printing distance be closer;
The cooling fan is 100% open when pumping back.

I hope this can help you.
-Keep your mind and try to test it. :)
-Everything will be fun!-Support all Getech printer.
-You can ask me the questions and I will kindly reply.
-Respect others is the best way you can get help!

Didi
Posts: 5
Joined: Tue Aug 27, 2019 4:52 pm

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by Didi » Tue Aug 27, 2019 5:37 pm

Thanks for your replie.

4mm and 5mm retraction has bad stringing. 6mm could be possible. I printed with 6mm at 20mm/s and 25mm/s. Both are not so good. See the picture in my first post.
How can i reduce the printing distance for the controller grip for example?
the fan is running 100% when travelling.

But it didn´t explains why two prints at the same settings looks totally different.

User avatar
William
Site Admin
Posts: 6340
Joined: Tue Jun 07, 2016 9:38 am

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by William » Tue Aug 27, 2019 5:44 pm

Hi, Stringing at its heart is molten filament oozing out of the nozzle during a fast travel move.
The hotter your print temperature, the more likely it is that oozing might occur.
and you can try to print by 5-10° at the hot end of the hot end.
-Keep your mind and try to test it. :)
-Everything will be fun!-Support all Getech printer.
-You can ask me the questions and I will kindly reply.
-Respect others is the best way you can get help!

Didi
Posts: 5
Joined: Tue Aug 27, 2019 4:52 pm

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by Didi » Tue Aug 27, 2019 5:51 pm

To choose the right temeprature i printed a heat tower and my print temperature is 195 degree. I think this is already low. I will try 190 degree. 185 is to low. The bridges are really bad at this temperature.

Didi
Posts: 5
Joined: Tue Aug 27, 2019 4:52 pm

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by Didi » Tue Aug 27, 2019 9:48 pm

I tried a lower temp. Same problem. I tried 4mm, 5mm and 6mm at 30 mm/s, and 6mm at 40 mm/s. Everytime i get a different result. Stringing is still bad.

Tommies
Posts: 13
Joined: Tue Jul 02, 2019 3:37 am

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by Tommies » Thu Aug 29, 2019 4:16 am


wotor
Posts: 51
Joined: Tue Dec 26, 2017 1:18 am

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by wotor » Thu Aug 29, 2019 7:48 am

Maybe someone has a good settings for PETG? I don't have problems with PLA but PETG is different story.

User avatar
William
Site Admin
Posts: 6340
Joined: Tue Jun 07, 2016 9:38 am

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by William » Thu Aug 29, 2019 9:15 am

wotor wrote:
Thu Aug 29, 2019 7:48 am
Maybe someone has a good settings for PETG? I don't have problems with PLA but PETG is different story.
Hi, about PETG,Bed Temperature: 75-90 °C, Extruder temperature: 230-250 °C,
you can refer to this :https://www.simplify3d.com/support/mate ... uide/petg/
I hope this can help you.
-Keep your mind and try to test it. :)
-Everything will be fun!-Support all Getech printer.
-You can ask me the questions and I will kindly reply.
-Respect others is the best way you can get help!

Didi
Posts: 5
Joined: Tue Aug 27, 2019 4:52 pm

Re: A10M Stringing / Oozing (Same Settings - Different Results)

Post by Didi » Thu Aug 29, 2019 12:17 pm

Hello,

Thanks for your reply.

I already know Your second link. Your first link recommended higher acceleration and travel speed and Retraction speed. Could You Tell me what are the Limits of the A10M?

Thanks